The main purpose preverting shorting outs between 2 windings. That is why i want clean Zn from both sides of PP barrier. Now i clean only partially prom inner side.
I add shrinkable tube on the barrier. Then spraying Zn 6 atm by plazma. But inner side has Zn still. So 2nd one i cut barrier.
But this also bad idea, because i have shorting outs on some samples(dust, particles of Zn on barrier).
So it's so hard now...😐

T10.JPG

IMG_8782.JPG

IMG_8796.JPG

IMG_8797.JPG

IMG_8798.JPG

IMG_8807.JPG

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...