Condensate and Aqueous Tank


Question

1 answer to this question

Recommended Posts

  • 0

I have seen this same thing many times. The overall surfaces are experiencing typical corrosion, which can be surprisingly difficult to prevent. The more extreme spots (especially the ones circled) were initiated by handling (bumped, scraped, dinged). The less extreme spots arise from debris that is no longer present, but facilitated and concentrated the chemical attach at those locations. These surfaces are not in the least unusual. Preventing this from happening requires considerable diligence and at least one of several available coatings. Note that if you coat a surface and it has any flaws, the attach will be much more pronounced at the flaws. See the attached paper.

1994 Corrosion in CS SW Piping .pdf

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Answer this question...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

  • Join Mechanical Engineering network

    Join us (login) to get full access : Please sign up to connect and participate.

    To download files...please login






×
×
  • Create New...